What is ALD Process ? Basic Characteristics of ALD Principles of ALD Technique ALD Cycle for Al2O3 Deposition Requirements for Precursors Types of ALD Reactors Closed System Chambers ALD Reactor ALD Applications Advantages & Limitations Summary
“ It’s a film deposition technique based on sequential use of self terminating surface reactions”
ALD is a CVD technique suitable for inorganic material layer as oxides, nitrides and some metals.
Perfect for deposition of very thin layers of the size of a monolayer.
Steps:◦ Self-terminating reaction of the first reactant (Reactant A)◦ Purge or evacuation to remove non-reacted reactant and by
products◦ Self-terminating reaction of the second reactant (Reactant B)◦ Purge
This is considered as one reaction cycle
The surface must be in a controlled state, e.g. heated Parameters to be adjusted:
◦ Reactants (precursors)◦ Substrate◦ Temperature
Self-termination of adsorption provides atomic scale control of the film thickness and ensures uniform coverage.
PrinciplesPrinciples of of ALDALD Technique TechniquePrinciplesPrinciples of of ALDALD Technique Technique
In air H2O vapor is adsorbed on most surfaces, forming a hydroxyl group. With silicon this forms: Si-O-H (s)
After placing the substrate in the reactor, Trimethyl Aluminum (TMA) is pulsed into the reaction chamber.
Tri-methylaluminumAl(CH3)3(g)
CH
HH
H
Al
O
Hydroxyl (OH)from surfaceadsorbed H2O
Methyl group(CH3)
Substrate surface (e.g. Si)
Al(CH3)3 (g) + : Si-O-H (s) :Si-O-Al(CH3)2 (s) + CH4
Trimethyl Aluminum (TMA) reacts with the adsorbed hydroxyl groups, producing methane as the reaction product
C
H
H
H
H
Al
O
Reaction ofTMA with OH
Methane reactionproduct CH4
H
HH
HH C
C
Substrate surface (e.g. Si)
C
HH
Al
O
Excess TMAMethane reactionproduct CH4
HH C
Trimethyl Aluminum (TMA) reacts with the adsorbed hydroxyl groups,until the surface is passivized. TMA does not react with itself, terminating the reaction to one layer. This causes the perfect uniformity of ALD. The excess TMA is pumped away with the methane reaction product.
Substrate surface (e.g. Si)
C
HH
Al
O
H2O
HH C
OHH
After the TMA and methane reaction product is pumped away, water vapor (H2O) is pulsed into the reaction chamber.
2 H2O (g) + :Si-O-Al(CH3)2 (s) : Si-O-Al(OH)2 (s) + 2 CH4
H
Al
O
O
H2O reacts with the dangling methyl groups & form aluminum-oxygen (Al-O) bridges and hydroxyl surface groups, waiting for a new TMA pulse.
Again Methane is the reaction product.
O
Al Al
New hydroxyl group
Oxygen bridges
Methane reaction product
Methane reaction product
H
Al
O
O
The reaction product methane is pumped away. Excess H2O vapor does not react with the hydroxyl surface groups, That caused perfect passivation to one atomic layer.
O O
Al Al
One TMA and one H2O vapor pulse form one cycle. Here three cycles are shown, with approximately 1 Angstrom per cycle. Each cycle including pulsing and pumping takes e.g. 3 sec.
O
H
Al Al Al
HH
OO
O OO OO
Al Al AlO O
O OO
Al Al AlO O
O OO
Al(CH3)3 (g) + :Al-O-H (s) :Al-O-Al(CH3)2 (s) + CH4
2 H2O (g) + :O-Al(CH3)2 (s) :Al-O-Al(OH)2 (s) + 2 CH4
Two reaction steps in each cycle:
Ligand Precursor◦ To prepare the surface for next layer, and define the kind of
material to growth i.e. H2O for oxides, N2 or NH3 for nitrides, etc.
Main Precursor (metallic precursor)◦ Highly reactive (usually this means volatile precursors)◦ Thermally stable◦ Full-fill the requirement for self terminating reaction◦ No self-decomposition◦ No etching of the film or substrate material◦ No dissolution into the film or substrate◦ Sufficient purity
14
Four main types of ALD reactorsFour main types of ALD reactors
Closed system chambersClosed system chambers Open system chambersOpen system chambers Semi-closed system chambersSemi-closed system chambers Semi-open system chambersSemi-open system chambers
15
Closed System ChambersClosed System Chambers The reaction chamber walls are designed to effect the The reaction chamber walls are designed to effect the
transport of the precursors.transport of the precursors.
• Open system chambersOpen system chambers• Semi-closed system chambersSemi-closed system chambers• Semi-open system chambersSemi-open system chambers
Schematic of a closed ALD system
Ref:Ref: "Technology Backgrounder: Atomic Layer Deposition," IC Knowledge LLC, 24 "Technology Backgrounder: Atomic Layer Deposition," IC Knowledge LLC, 24 April 06. <April 06. <www.icknowledge.com/misc_technology/Atomic%20Layer%20Deposition%20Briefing.pdf>.>.
16
The Verano 5500™A 300-mm ALD system by Aviza Technology, Inc [2].
Process Temperature [1]
[1] [1]
11 "Technology Backgrounder: Atomic Layer Deposition," IC Knowledge LLC, 24 "Technology Backgrounder: Atomic Layer Deposition," IC Knowledge LLC, 24 April 06. <April 06. <www.icknowledge.com/misc_technology/Atomic%20Layer%20Deposition%20Briefing.pdf>>
22 ”Atomic Layer Deposition," Aviza Technology. 26 ”Atomic Layer Deposition," Aviza Technology. 26 April 06. <April 06. <http://www.avizatechnology.com/products/verano.shtml>.>.
Semi & Nanoelectronics Coatings on Polymers Protective Coatings Magnetic Heads Thin Film Electroluminescent Displays (TFELs) MEMS Nanostructures Chemical Solar Cell
18
ALD Highly reactive precursors Precursors react separately on
the substrate Precursors must not
decompose at process temperature
Uniformity ensured by the saturation mechanism
Thickness control by counting the number of reaction cycles
Surplus precursor dosing acceptable
CVD Less reactive precursors Precursors react at the same time
on the substrate Precursors can decompose at
process temperature Uniformity requires uniform flux of
reactant and temperature Thickness control by precise
process control and monitoring Precursor dosing important
Self-limiting growth process Precise film thickness control by the number of deposition cycles No need to control reactant flux homogeneity Excellent uniformity and conformity Large-area and batch capability Dense, uniform, homogeneous and pinhole-free films Atomic level composition control Good reproducibility and straightforward scale-up Surface exchange reactions by separate dosing of reactants
Expensive equipment Low Effective Deposition Rate Critical adjustment of the flow: too much flow => clogging of valves too low flow => under-performance
Summary
Its unique self-limiting growth mechanism which gives perfect conformality and uniformity.
Easy and accurate thickness control down to an atomic layer level. Closed System Chambers ALD Reactor is one of the mostly used one. ALD is a slow method Expensive equipment & Low Effective Deposition Rate ALD has many applications in the field of Nanoelectronics, Optical,
MEMS, Nanostructures & in Solar cell