+ All Categories
Home > Documents > Avestruz - Majorfe · Avestruz collection Technical Specifications Composition % SEDE ESPUMAS...

Avestruz - Majorfe · Avestruz collection Technical Specifications Composition % SEDE ESPUMAS...

Date post: 08-Jun-2020
Category:
Upload: others
View: 2 times
Download: 0 times
Share this document with a friend
1
Polyester Polyviny Chloride Polyurethane Weight Avestruz collection Technical Specifications Composition % SEDE ESPUMAS [email protected] [email protected] www.majorfe.com NOTE Due to dying process, some colors could present slightly difference between the col. swatch display on the catalogue, and the one expected. MAJORFE, appeal for YOUR revalidation of the col. Exhibit on the catalogue, in result of eventuality failures in the elaboration of the catalogues. Certain clothing and accessories dyes (such as those used in denim jeans), may migrate to lighter colors. This phenomenon is increase by humidity and temperature, and is irreversible. MAJORFE, will not assume responsibility for the dye transfer caused by external contaminants and possible permanent staining caused by this phenomenon. * This term and any corresponding data refer to the typical performance in the specic tests indicated and should not be construed to imply the behavior of this or any other material under actual re condictions. Unit CARE AND CLEANING - The vinyl should be cleaned periodically in order to maintain its appearance and prevent build-up of dirt and contaminants. - Any stain, spills, or soiling should be cleaned up promptly to prevent the possibility of permanent staining. - Vinyl fabrics treated with Permablok3 require a minimum of maintenance to retain their good looks. Use soft soapy solutions or special cleaning products for vinyl fabrics to remove stains on the surface of the material. Remove only with a damp with cloth. - Lacquers. Strong cleaners. Detergents. Xylene-Based solutions, Acetone or MEK cause immediate damage and contribute to the deterioration of the material. The use of such cleaners is at the owner´s risk. Thickness Tensile Strenght Tear Strenght Flexing Endurance Abrasion Resistence % % 23 2 75 Elongation at break Along Value Test Types Aspect Unit Norm Standart Color Fastness to rubbing Across Light Fastness Light Colors Dark Colors Along Across Along Across at 23ºC Wet Dry gr/m2 mm N N N N % % FLX RUB GS GS BW BW 600 +/- 5% 1,40 +/- 5% min.360 min.480 min.35 min.60 min.110 +/-20% min.80 +/-20% min.80000 min.22000 min.5 min.5 min.4 min.5 ISO 2286-2 ISO 2286-3 ISO 1421 ISO 1421 ISO 4674-2 ISO 4674-2 ISO 1421 ISO 1421 ISO 5402 DIN 53863 ISO 105X12 ISO 105X12 ISO 105B02 ISO 105B02
Transcript
Page 1: Avestruz - Majorfe · Avestruz collection Technical Specifications Composition % SEDE ESPUMAS encomendas@majorfe.com espumas@majorfe.com NOTE Due to dying process, some colors could

Polyester

Polyviny Chloride

Polyurethane

Weight

Avestruz collectionTechnical Specifications

Composition

%

SEDE ESPUMAS

[email protected] [email protected] www.majorfe.com

NOTEDue to dying process, some colors could present slightly difference between the col. swatch display on the catalogue, and the one expected.

MAJORFE, appeal for YOUR revalidation of the col. Exhibit on the catalogue, in result of eventuality failures in the elaboration of the catalogues.

Certain clothing and accessories dyes (such as those used in denim jeans), may migrate to lighter colors. This phenomenon is increase by humidity and

temperature, and is irreversible. MAJORFE, will not assume responsibility for the dye transfer caused by external contaminants and possible permanent

staining caused by this phenomenon.

* This term and any corresponding data refer to the typical performance in the specic tests indicated and should not be construed to imply the behavior

of this or any other material under actual re condictions.

Unit

CARE AND CLEANING- The vinyl should be cleaned periodically in order to maintain its appearance and prevent build-up of dirt and contaminants.

- Any stain, spills, or soiling should be cleaned up promptly to prevent the possibility of permanent staining.

- Vinyl fabrics treated with Permablok3 require a minimum of maintenance to retain their good looks. Use soft soapy solutions or special cleaning

products for vinyl fabrics to remove stains on the surface of the material. Remove only with a damp with cloth.

- Lacquers. Strong cleaners. Detergents. Xylene-Based solutions, Acetone or MEK cause immediate damage and contribute to the deterioration of the

material. The use of such cleaners is at the owner´s risk.

Thickness

Tensile Strenght

Tear Strenght

Flexing Endurance

Abrasion Resistence

%

%

23

2

75

Elongation at break

Along

Value

Test Types Aspect Unit Norm Standart

Color Fastness to rubbing

Across

Light Fastness Light ColorsDark Colors

AlongAcross

AlongAcross

at 23ºC

WetDry

gr/m2

mm

NN

NN

%%

FLX

RUBGSGSBWBW

600 +/- 5%

1,40 +/- 5%

min.360min.480

min.35min.60

min.110 +/-20%min.80 +/-20%

min.80000

min.22000

min.5min.5

min.4min.5

ISO 2286-2

ISO 2286-3

ISO 1421ISO 1421

ISO 4674-2ISO 4674-2

ISO 1421ISO 1421

ISO 5402

DIN 53863ISO 105X12ISO 105X12ISO 105B02ISO 105B02