Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated...

Date post: 29-Mar-2015
Category:
Upload: dwayne-sopp
View: 217 times
Download: 2 times
Share this document with a friend
Popular Tags:
25
Barcelona, 20/08/2011
Transcript
Page 1: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

Barcelona, 20/08/2011

Page 2: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

INTRODUCTION

• More than 25% of the existing housing moistures are

originated on the roof. Mainly caused by the lack

waterproofing solution or the failure.

• A roof is a protection element exposed to atmospheric

agents (rain, ice, snow, solar radiation, pollution, etc.)

Barcelona, 20/08/2011

Page 3: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

ROOF TYPES

• Following its shape:

Flat or bent skirt, flat or pitched, simple or double bent, etc.

• Following its constructive elements:

Homogeneous (one layer), heterogeneous (multiple layers)

• Following its protection or finishing:

Concrete, tiles, stoneware, panels, etc.

• Following its uses:

Trafficable (not vehicular), non trafficable or green roofs.

Barcelona, 20/08/2011

Page 4: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

WATERPROOFING TYPES

The most important characteristic from a waterproofing system is its sealing power against atmospheric and pollution agents.

Most common types:

Waterproofing sheets (bituminous or synthetic)Metal sheets (folding and moldable)Metal deck- Metal panelsBig elements with sealed jointsOverlap elements (tiles, slates) Liquid ( bitumen emulsions, acrylic emulsions, epoxy, PU, polyuria, etc.)

Barcelona, 20/08/2011

Page 5: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

PATHOLOGICAL AGENTS

• RAIN• WATER CONDENSATION OR DEW• HAIL• WIND• FREEZE-THAW • SOLAR RADIATION• POLLUTION

Barcelona, 20/08/2011

Page 6: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

PRODUCT DESCRIPTION

•Elastic coating based on an acrylic copolymer emulsion

Barcelona, 20/08/2011

Page 7: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

TECHNICAL PROPERTIES

• Adaptive liquid membrane for structures with irregular geometry.

• Monolithic membrane without joints or overlaps and securely

attached.

• Water based. Thinner, tar or any asphalt derivate product free.

• Easy to apply: single-component, roller, brush or airless spray.

• 100% waterproof.

• Breathable to water vapor. I allows the support to breath.

Barcelona, 20/08/2011

Page 8: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

TECHNICAL PROPERTIES

• Very good elongation properties. High absorption capacity to the

roof movements caused by temperature changes or settlement.

• Great endurance to atmospheric agents.

• Formulated to comply with UNE 53.413 norm for flexible

coatings without reinforcement.

• Environmentally friendly, complies with Directive 2004/42/CE in

relation with Volatile organic compounds (VOC).

Barcelona, 20/08/2011

Page 9: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

USES

• Specially indicated for waterproofing of external concrete surfaces,

precast concrete, bitumen waterproofing, tiles, asbestos cement,

projected PU foam, expanded polyethylene and wood (balconies and

terraces), roofs, vaults, balconies, gutters, pots, etc.

• In liquid applied waterproofing for non trafficable balconies and terraces,

for private use when reinforced with geotextile IMPERTEXSA A-50.

• Protection of polyurethane foam insulation.

Barcelona, 20/08/2011

Page 10: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

USES

• In adaptive liquid waterproofing coating for structures with irregular

geometry and protective coating on vertical walls.

• Provides a monolithic continuous elastic and flexible coating without joints

or overlaps.

• In repair and rehabilitation waterproofing work over concrete, mortar,

asbestos cement, non glass ceramic tiles, tiles, wood, etc.

• Protection of concrete structures in marine environment.

Barcelona, 20/08/2011

Page 11: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

TECHNICAL DATA

Barcelona, 20/08/2011

Characteristics Value

Aspect Semi matt

Color White, blue, red, grey, green and terracotta.

Viscosity 120.000 centipoises

Solid Volume 42 – 45%

Consumption 2 kilos / m² , in two or three layers

Tack 3 hours at 20º C

Elongation at Break 400 – 600%

Cold bending No cracks between – 5ºC and 180°C

Washability > 10.000 cycles following UNE-48284

VOC Complies with Directive 2004/42/CE, Annex I subclass c) 3,9 – 4,1 g/l depending on the color (40g/l maximum 2010)

Page 12: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION

• Application method : roller, brush or airless spray.• Dilution : 0 to 5%• Diluent and cleaning : Water• Repainting time: 12 - 24 hours at 20º C

– Can be repainted after cleaning the existing coating as much as needed.

Application conditions: Working temperatures must be above 10 °C and below 35 °. RH below

80 %. Temperatures of support and coating must be within the application

conditions too.

Barcelona, 20/08/2011

Page 13: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION

Support :•The concrete structures must be cured for 28 days.•The surface to be treated should be clean of grease, oil, curing chemicals, dust and dirt. •IMPERTEXSA can be applied directly on wet substrate following sealing procedure. •Eliminate surface irregularities. Do not apply on loose, dusty, unclean substrates which are unacceptable to receive the coating. If required use mechanical or manual tools to clean the support.•Resurface and seal the cracks with polyurethane caulk, reinforced with ROOFTEX FLEECE 80 wherever necessary.•Treat the expansion joints (according to standards) and seal with polyurethane caulk.

Barcelona, 20/08/2011

Page 14: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION

Support :•We recommend using a thin geotextile interlayer to control the film thickness and uniformity.

Sealing:•Apply on layer of IMPERTEXSA CUBIERTAS 20% diluted with water. Drying time 2 to 4 hours at 20º C.Finishing:•Apply two layers of IMPERTEXSA CUBIERTAS without diluting. Drying time between layers is 12 hours.

Barcelona, 20/08/2011

Page 15: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

PRECAUTIONS

• Don’t apply IMPERTEXSA CUBIERTAS if rain is forecasted during drying

time, on cloudy days or during maximum insolation hours.

• Drying time and repainting time may vary following weather conditions.

• Apply on surfaces with enough slope to avoid stagnant water.

• This product is not recommended for trafficable areas, although temporary

pedestrian accessibility is allowed for maintenance jobs.

Barcelona, 20/08/2011

Page 16: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

PRECAUTIONS

• Avoid direct exposition to sun of the containers.

• For a correct waterproofing, we recommend to cross layers between first

and second hand, reaching a better distribution of the coating and

correctly regularize the consumption.

• On roof waterproofing, parapet (walls) must be painted with a minimum

high of 15 cm.

• Don’t use brackish water, chemically polluted, cloudy or calcareous in

excess. It could be alter the product properties.• Storage of the containers must be protected from frost, prolonged

exposure to sunlight and high temperatures.

Barcelona, 20/08/2011

Page 17: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

PACKING

• 20 and 5 kilos drums.

• Colors: White, blue, red, terracotta, green and grey.

• Recommended maximum storage time: 1 year at 25 º C in their respective

containers.

Barcelona, 20/08/2011

Page 18: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

SAFETY

• Water based product. Each container has a safety label with instructions

that must be observed. National an local safety regulation must also be

respected.

• Avoid inhalation of vapor or direct contact of the painting with skin and

eyes. If applied on enclosed rooms, force ventilation is required.

• Use personal protective equipment..

• IMPERTEXA CUBIERTAS is free of nonylphenols, formaldehydes,

thinners, tar, asphalt or chloride plasticizers.

Barcelona, 20/08/2011

Page 19: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 20: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 21: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 22: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 23: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 24: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.

APPLICATION EXEMPLES

Barcelona, 20/08/2011

Page 25: Barcelona, 20/08/2011. INTRODUCTION More than 25% of the existing housing moistures are originated on the roof. Mainly caused by the lack waterproofing.