40
ILLUSTRATIONS REPAIRING OF STRUCTURES AVINASH KUMAR GUPTA TRAINING INSTITUTE CCW AIR APRIL 2017
Transcript
Page 1: Illustrations. repairing of structures

ILLUSTRATIONS

REPAIRING OF STRUCTURES AVINASH KUMAR GUPTA

TRAINING INSTITUTE

CCW AIR

APRIL 2017

Page 2: Illustrations. repairing of structures

Strengthening Of columns

• Section Enlargement by jacketing.• Apply specified bond coat on existing column.• Bond coat of sunepoxy 368• M-25 or higher grade of concrete.

Page 3: Illustrations. repairing of structures
Page 4: Illustrations. repairing of structures

Strengthening of Beams• Section enlargement with micro concrete• Shotcrete self compaction concrete• Increased flexure strength by enlarging

compression zone and additional reinforcement in tension.

• Increased shear strength by fixing of stirrup with epoxy and quartz sand mortar as specified.

• MS Plate bonding• High strength fiber fabric wrap technique.

Page 5: Illustrations. repairing of structures
Page 6: Illustrations. repairing of structures

Strengthening Of Slab

• Provide overlays in case of negative moment deficiency.

• Provide underlay in case of positive moment deficiency.

• Increase in stiffness and control of deflection.• Slabs are safe in shear.

Page 7: Illustrations. repairing of structures
Page 8: Illustrations. repairing of structures

STICHING of walls/slab cracks

• Concrete and masonry weak in tension.• Crack indicate tensile failure of material• Insert U shaped MS bars in the holes and span

across the crack.• Grouting the holes with either epoxy or non

shrink grout.(non moving cracks)• Active cracks are to be filled with flexible

materials like poly- sulphides, bituminous fillers.

Page 9: Illustrations. repairing of structures
Page 10: Illustrations. repairing of structures
Page 11: Illustrations. repairing of structures

BEAM AND COLUMN REPAIR BYGUNITE/SHOTCRETE

Page 12: Illustrations. repairing of structures

TREATMENT OF DEPRESSED FLOOR IN TOILET/KITCHEN

• Remove all materials and expose the pipes.• Test the water supply pipes and drainage pipes

for leakages using pressure applying methods.• Provide 40 mm dia GI spout and CC sloped

flooring with water proofing compound. • Provide 12 mm thick cement plaster (1:3) with

water proofing on the vertical walls • Provide two coats of bitumen(85/25)in the

sunken portion.

Page 13: Illustrations. repairing of structures
Page 14: Illustrations. repairing of structures

Column Beam Junction

Page 15: Illustrations. repairing of structures

Repairs at Beam column junction

Page 16: Illustrations. repairing of structures

Beam Column Junction

Page 17: Illustrations. repairing of structures

COOROSION IN BARS .RCC STRUCTURE

Page 18: Illustrations. repairing of structures

CORODED BARS REPAIR• Remove all defective concrete and expose

corroded reinforcing bars to their full circumference.

• Remove the corrosion from the bars until the shine.

• Apply anti corrosive protective passivating coat to protect re –bars.

• Patch with repair mortar or concrete and resurface to required thickness.

• Apply protective coating and follow up with decorative painting.

Page 19: Illustrations. repairing of structures

JACKETING

Page 20: Illustrations. repairing of structures

Column repairs

Page 21: Illustrations. repairing of structures

GROUTING

Page 22: Illustrations. repairing of structures

Beam Strengthening

Page 23: Illustrations. repairing of structures

REPAIR STRATEGY

• Remove all unsound concrete at spalled ,cracked and hollow sounding areas.

• Expose the full corroded rebars to further depth.• Remove corrosion by approved manual method

or by sand blasting.• Treat rebars by a passivating material.• Shotcreting, microconcreting• Curing and top coat of alkyd to prevent ingress of

deleterious gases.

Page 24: Illustrations. repairing of structures

Beam Repairs

Page 25: Illustrations. repairing of structures

CRACK FORMATION, IDENTIFY THE CAUSE

Page 26: Illustrations. repairing of structures

Brick wall Column Junction

Page 27: Illustrations. repairing of structures

Jacketing upto foundation level

Page 28: Illustrations. repairing of structures

Over Head Tank repair

Page 29: Illustrations. repairing of structures
Page 30: Illustrations. repairing of structures

Bridge Repair

Page 31: Illustrations. repairing of structures

Roof Repair

Page 32: Illustrations. repairing of structures

Water proofing of roofs

• Remove existing treatment.• Number of rain water pipes to be increased.• Mark surface cracks. Inject polymer modified cement

slurry through nipples along crack lines.• Regarding.• Apply two coats of polymer modified cement slurry

with 20% polymer.• Apply 20 mm thick polymer modified non shrink

cement plaster with 300 X300 square thread identation.

• Curing and ponding to check adequacy.

Page 33: Illustrations. repairing of structures

FILLING CRACKS

Page 34: Illustrations. repairing of structures

Filling Cracks

Page 35: Illustrations. repairing of structures

Basement Repair

Page 36: Illustrations. repairing of structures

Leak Reapair , Rubber based polymer

Page 37: Illustrations. repairing of structures

DOME REPAIR

Page 38: Illustrations. repairing of structures

DOME REPAIR, External surface

• Remove old plaster.• Fix grouting nipples and inject cement based

non shrink slurry.• Provide first layer of Ferrocement.• Lay second layer and level upto required level.• Cure for 14 days.• Apply anti carbonation treatment in two

layers.

Page 39: Illustrations. repairing of structures

Dome repair , Internal surface

• Remove old plaster and clean joints wth brushes.• Remove corroded steel and replace it.• Pack with non shrink concrete.• Repack all exposed masonry joints with non

shrink cement sand mortar. Pressure grout with nozzles at the dome junction with bottom drum.

• Provide specified layer of ferrocement.• Cure for 10 days • Apply two coats of polymer cement water