Cara membuat WPS dan PQR
Popular Tags:
9
Victor Rizal Filosofi Imam Khoirul Rohmat
Transcript
Page 1: Inspeksi Pengelasan

Victor Rizal FilosofiImam Khoirul Rohmat

Page 2: Inspeksi Pengelasan

Material (QW-403) Base Metal A 53 Pipe P-No. 1 Group No. 1 Diameter pipa 6,5” tebal 1/3”

Filler Metal (QW-404) Spec. No SFA-5.1 AWS No. E7016 LB Diameter 2,6 dan 3,2

Posisi Pengelasan (QW-405) 1 G pipa

Joint Design (QW-402) V Grove

Page 3: Inspeksi Pengelasan

Speed Rate Root = 2 mm/dtk

Pas = 2,2 mm/dtk Capping = 2 mm/dtk

Arus Root = 60Ampere Pas = 80 Ampere Capping = 90 Ampere

Page 4: Inspeksi Pengelasan

Vissual

X-Ray

Page 5: Inspeksi Pengelasan

Dimensi Las (Welding Gauge) Root tertinggi = 4 mm Root Terendah = 0 mm Capping Tertinggi= 3 mm Capping Terendah = 1,5 mm Lebar Capping = 10mm Cacat Under Cut IP Akar terlalu tinggi

Page 6: Inspeksi Pengelasan

Screen Lead = Front n’ back Thick = 0.125 mm

Film Manufacturer = Kodak Type = AA 100 Dimension = 4 x 10 inch

Sumber Radiasi Tegangan 190 KV Time 1 menit 2 detik

Page 7: Inspeksi Pengelasan

Technique Exposure = Single Wall Viewing = Single Image Min. SFD = 80, 8 mm Ac. SFD = 600 mm

IQI Wire Side – B no.7 Placement = Film Side

Marker Placement Film Side

Page 8: Inspeksi Pengelasan

Range of Density Acceptable2 – 4

Density Dark = 3,8 IQI = 3,4 Bright = 1,75

Defect Incomplete Penetration Incomplate Fussion Undercut Slag inclution

Page 9: Inspeksi Pengelasan

04/08/23 9