Home > Documents > strate at 4.0 mils wft (wet film thickness) and would dry at approximately 1.5 mils dft (dry film...

strate at 4.0 mils wft (wet film thickness) and would dry at approximately 1.5 mils dft (dry film...

Date post: 26-Mar-2020
Category:
Upload: others
View: 2 times
Download: 0 times
Share this document with a friend
5
Transcript
Page 1: strate at 4.0 mils wft (wet film thickness) and would dry at approximately 1.5 mils dft (dry film thickness) per coat. The full procedure was performed within one eight hour shift.
Page 2: strate at 4.0 mils wft (wet film thickness) and would dry at approximately 1.5 mils dft (dry film thickness) per coat. The full procedure was performed within one eight hour shift.
Page 3: strate at 4.0 mils wft (wet film thickness) and would dry at approximately 1.5 mils dft (dry film thickness) per coat. The full procedure was performed within one eight hour shift.