+ All Categories
Transcript
Page 1: Radiographic Interpreter: Weld Defect Exercise Part 1

ASNT RT LEVEL 2

IN-HOUSE TRAINING

AL-USWAH INSPEKSITAMA

NDT TRAINING CENTER

Jl. Raya Natar No. 55, Pasar Lama Natar Lampung Selatan

Telp. 0721-91025 / 081369255454 E-mail: [email protected]

Page 2: Radiographic Interpreter: Weld Defect Exercise Part 1

X1

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 3: Radiographic Interpreter: Weld Defect Exercise Part 1

X2

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 4: Radiographic Interpreter: Weld Defect Exercise Part 1

X3

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 5: Radiographic Interpreter: Weld Defect Exercise Part 1

X4

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 6: Radiographic Interpreter: Weld Defect Exercise Part 1

X5

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 7: Radiographic Interpreter: Weld Defect Exercise Part 1

X6

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 8: Radiographic Interpreter: Weld Defect Exercise Part 1

X7

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 9: Radiographic Interpreter: Weld Defect Exercise Part 1

X8

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 10: Radiographic Interpreter: Weld Defect Exercise Part 1

X9

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 11: Radiographic Interpreter: Weld Defect Exercise Part 1

X10

AL-USWAH INSPEKSITAMA NDT TRAINING CENTER

Page 12: Radiographic Interpreter: Weld Defect Exercise Part 1

JAWABAN

� X1 No Defect

� X2 Elongated Cavity

� X3 Distributed Porosity

� X4 Clustered Porosity

� X5 Linear Porosity

� X6 Linear Slag Inclusion

� X7 Continuous Undercut

� X8 Incomplete Penetration

� X9 Worm Hole

� X10 Root Fusion