Defects In Crystalline Materials.

Page 3: defects

Presented by, Muhammad Naveed Ch. Shafiq Ahmad. Asif Iqbal. Husnain Riaz.

Page 4: defects

Defects In Crystalline Materials.

Metals, many ceramics and some polymers are crystalline.

Real crystals contain various types of imperfections.

Many of the important properties of materials are due to the presence of these imperfections.

Page 5: defects

Types Of Defects.

Defects are categorized as:1) Point defects.2) Surface defects.3) Volume defects.4) Line defects.

Page 6: defects

Point Defects.

All the atoms in a perfect lattice are at specific atomic site.

In a pure metal two types of point defects are possible.

1) Vacancies.2) Interstitial point defects.

Page 7: defects

Vacancies.

Vacant atomic sites in a structure.

Due to plastic deformation & high energy particle irradiation.

Page 8: defects

Interstitial Point Defects.

“Extra" atoms positioned between atomic sites.

Due to plastic deformation & high energy particle irradiation Interstitial

atom

distortionof planes

Page 9: defects

Extrinsic Point Defects.

Introduction of outsider atom. They play an important role in physical &

mechanical properties. Impurity atom can take two different sites

in crystal. Substitutional or Interstitial.

Page 10: defects

vacancy Interstitialimpurity

Substitutionalimpurity

Point Defects

Page 11: defects

In metallic solids defects are not so important but in ionic solids presence of a vacant site (e.g. in NaCl), changes the electrical properties.

Page 12: defects

In order to conserve the overall neutral charge vacancy must be occurred either in pairs of opposite sign forming die-vacancies called Schottky defects.

In association of the interstitial of same ion called Frenkel defects.

Schottky & Frenkel Defects

Page 13: defects

Frenkel defect

Schottky defect

Defects in ionic solids

Cation vacancy+

cation interstitial

Cation vacancy+

anion vacancy

Page 14: defects

Stacking Faults.

Stacking fault is a planner defect and formed when regular sequence of stacking is disturbed.

Stacking faults are not may observed In planes where the stacking sequence is ABABAB….because there is no alternative site for “A” layer other than resting on a “B” layer of vice versa.

In ABCABABC….layers it is visible.

Page 15: defects

AB

C

Page 16: defects

Types Of Stacking Faults.

1) Intrinsic stacking faults.2) Extrinsic stacking faults.

Page 17: defects

Intrinsic Stacking Faults.

Removal of a layer from an arranged sequence layer.

E.g. CBACBA…..becomes CBABAC….

Page 18: defects

Extrinsic Stacking Faults.

Addition of layer to the arranged sequence layer.

E.g. BACBAC….becomes BACABAC…

Page 19: defects

Grain Boundaries.

A Grain Boundary is a general planar defect that separates regions of different crystalline orientation (i.e. grains) within a polycrystalline solid.

The atoms in the grain boundary will not be in perfect crystalline arrangement

Page 20: defects

Grain Boundaries Cont...

Grain boundaries are usually the result of uneven growth when the solid is crystallizing.